High frequency acoustic excitation downstream of pressure reducing device and potential of downstream piping failure on Acoustic Induced Vibration (AIV) has raised concern in many plant design. Earlier post "Extra Attention to Common Point and Similarity on AIV Failure" has discussed the common points and similarity of AIV such as typical failure location, system experienced failure in the past, failure time & period and Mach no. An engineer assessing AIV shall pay extra attention in these factors.
Sound Power Level (PWL) is the acoustic energy generated by a pressure reduction device. There are several ways to assess the adequacy of the piping to resist AIV fatigue. One of the way to ensure piping downstream of pressure reducing device sufficiently strong to resist AIV fatigue is to ensure the PWL allowable limit of downstream piping higher than the PWL generated by the pressure reducing device. Refer to "Sound Power Level (PWL) Prediction" for equation in prediction PWL.
A piping will have it stiffness and resistivity against vibration. It is very much subject to piping diameter, material properties, wall thickness, distribution of masses, pipe support, etc. Allowable sound power level and/or dynamic stress of piping can be a measurement of this resistivity of piping against excitation due to AIV. Several allowable PWL curves for piping which derived from different method i.e. "D-method", "D/t-method ", "E-method", etc have been used. Besides PWL related method, there are other method i.e. "Dynamic stress method", "Likelihood of Failure (LOF) method", etc which adopting allowable stress level also been used.
"D-Method"
Based on data available in Carucci & Mueller (1982) studies, "No failure" and "Failure" points have been plotted in the following chart.
Note :
1) A "failure" point (0.3m, 165dB) is below curve. It is failed on bad welding. No further failure after good welding.
2) Red point are "failure" point and Blue point are "No failure" point
3) May be used for 0.2m < D < 0.9m. Use at risk for D < 0.2m and D > 0.9m
PWL Limit Equation For "D-method"
A PWL limt line has been derived from above data and following equation representing this line.
where
PWLlimit = Maximum allowable PWL at Pipe diameter D meter, (dB)
D = Pipe diameter, (m)
This line may be used to assess potential failure of piping downstream of pressure reducing device. Any point above the line potentially fail on AIV, piping treatment or redesign required to minimise the risk of AIV failure. This will be discussed in future...
Related Topic
- Tips on Succession in FREE Subscription
- Subscribes to FREE Hydrocarbon Processing
High frequency acoustic excitation downstream of pressure reducing device and potential of downstream piping failure on Acoustic Induced Vibration (AIV) has raised concern in many plant design. Earlier post "Extra Attention to Common Point and Similarity on AIV Failure" has discussed the common points and similarity of AIV such as typical failure location, system experienced failure in the past, failure time & period and Mach no. An engineer assessing AIV shall pay extra attention in these factors.
Sound Power Level (PWL) is the acoustic energy generated by a pressure reduction device. There are several ways to assess the adequacy of the piping to resist AIV fatigue. One of the way to ensure piping downstream of pressure reducing device sufficiently strong to resist AIV fatigue is to ensure the PWL allowable limit of downstream piping higher than the PWL generated by the pressure reducing device. Refer to "Sound Power Level (PWL) Prediction" for equation in prediction PWL.
A piping will have it stiffness and resistivity against vibration. It is very much subject to piping diameter, material properties, wall thickness, distribution of masses, pipe support, etc. Allowable sound power level and/or dynamic stress of piping can be a measurement of this resistivity of piping against excitation due to AIV. Several allowable PWL curves for piping which derived from different method i.e. "D-method", "D/t-method ", "E-method", etc have been used. Besides PWL related method, there are other method i.e. "Dynamic stress method", "Likelihood of Failure (LOF) method", etc which adopting allowable stress level also been used.
"D-Method"
Based on data available in Carucci & Mueller (1982) studies, "No failure" and "Failure" points have been plotted in the following chart.
Note :
1) A "failure" point (0.3m, 165dB) is below curve. It is failed on bad welding. No further failure after good welding.
2) Red point are "failure" point and Blue point are "No failure" point
3) May be used for 0.2m < D < 0.9m. Use at risk for D < 0.2m and D > 0.9m
PWL Limit Equation For "D-method"
A PWL limt line has been derived from above data and following equation representing this line.
PWLlimit = 156.8 - 9.8 Ln (D)
where
PWLlimit = Maximum allowable PWL at Pipe diameter D meter, (dB)
D = Pipe diameter, (m)
This line may be used to assess potential failure of piping downstream of pressure reducing device. Any point above the line potentially fail on AIV, piping treatment or redesign required to minimise the risk of AIV failure. This will be discussed in future...
Related Topic
- Extra Attention to Common Point and Similarity on AIV Failure
- Piping Excitation When Expose to Acoustic Energy
- Acoustic Induced Vibration (AIV) Fatigue
- Sound Power Level (PWL) Prediction from AIV Aspect
- Several Criteria and Constraints for Flare Network - Piping
- Flow Element (FE) Upstream or Downstream of Control Valve (CV) ?
0 Comments:
Post a Comment
Let us know your opinion !!! You can use some HTML tags, such as <b>, <i>, <a>
Subscribe to Post Comments [Atom]
Home:
<< Home